Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 847 Nylon 6, Film Grade

Category Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 847 Nylon 6, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A very high impact, low flexural modulus Nylon 6 resin for molding or extrusion. Outstanding low temperature properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ATSM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 0.690 GPa
100 ksi
ASTM D790
Izod Impact, Notched 10.7 J/cm
20.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C
124 °F
ASTM D648