Material Notes:
Basic Nylon 6 medium viscosity, with high residual monomer. Highly flexible and high strength, particularly suited for monofilament extrusion.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Water Absorption 1.9 %
1.9 %
24 hrs; ASTM D570
Water Absorption at Saturation 9.6 %
9.6 %
ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 79.0 MPa
11500 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 62.0 MPa
8990 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D3418