Material Notes:
High impact, black, economy grade. Also available as: 827SB - Heat Stabilized, Black and 827SH - Heat Stabilized & UV Stabilized for Weatherability, Black.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 7.48 J/cm
14.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648