Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 69MG Nylon 66, Glass/Mineral reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 69MG Nylon 66, Glass/Mineral reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A glass/mineral reinforced high flow Nylon 66 with exceptional dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ATSM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Modulus 3.60 GPa
522 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved