Material Notes:
A reinforced modified, platable nylon with high impact and excellent dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ATSM D638
Elongation at Yield 18 %
18 %
ASTM D638
Flexural Modulus 3.70 GPa
537 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648