Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 630 Nylon 6, General Purpose

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 630 Nylon 6, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose Nylon 6 resin for injection molding.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.6 %
1.6 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH; ASTM D570
Water Absorption at Saturation 9.6 %
9.6 %
ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 75.0 MPa
10900 psi
ATSM D638
Elongation at Break 65 %
65 %
ASTM D638
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 179 °C
354 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D648