Ashley Polymers Ashlene® 528L-50LG Nylon 66, 50% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528L-50LG Nylon 66, 50% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 255 MPa
37000 psi
ATSM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 2.99 J/cm
5.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 259 °C
498 °F
ASTM D648