Ashley Polymers Ashlene® 526 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 526 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact Nylon 66 with good stiffness and good low temperature properties for injection molding. Values shown are for Natural. Colors may change some properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Ultimate 68.0 MPa
9860 psi
ATSM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 1.92 J/cm
3.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418