Ashley Polymers Ashlene® 521/522 Nylon 66, TiO2 Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 521/522 Nylon 66, TiO2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose grades of Nylon 66 containing 0.2% and 1.0% TiO2 respectively.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 66.0 MPa
9570 psi
ATSM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648