Material Notes:
A general purpose Nylon 66 resin, black, utility grade.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ATSM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 211 °C
412 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648