Material Notes:
A general purpose, high viscosity, natural.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.22 %
0.22 %
ASTM D570
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 16 g/10 min
16 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ATSM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Shear Strength 55.0 MPa
7980 psi
ASTM D732
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
ASTM D150