Ashley Polymers Ashlene® 1410B Polycarbonate, 8-10% Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 1410B Polycarbonate, 8-10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A rigid black polycarbonate, for applications requiring superior dimensional stability and overall toughness. Contains 8-10% glass reinforcement. Also available: 1413B, UV stabilized.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ATSM D638
Elongation at Break 11.5 %
11.5 %
ASTM D638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256