Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machine feed and easy mold release and has an Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thickAvailability:Asia PacificEuropeNorth AmericaAdditive:Flame RetardantLubricant Features: DuctileGood Mold ReleaseHalogen FreeIgnition ResistantLow DensityLubricatedUses:AppliancesAutomotive ElectronicsBobbinsConnectorsElectrical HousingElectrical PartsElectrical/Electronic ApplicationsFastenersIndustrial ApplicationsLighting ApplicationsLiving HingesPrinted Circuit BoardsSwitchesAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Diameter 2.00 mm
0.0090 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Diameter 2.00 mm
0.0060 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO 527-2
Elongation at Break 5.0 %
5.0 %
ISO 527-2
Flexural Strength 39.0 MPa
5660 psi
ISO 178
Flexural Modulus 1.35 GPa
196 ksi
ISO 178