Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, good toughness, a high melt point, abrasion resistance with good surface lubricity, and excellent resistance to many chemicals. Vydyne 21SPC1 resin has an external lubricant for improved machine feed and an internal lubricant for improved mold release. Typical Applications/End Uses: Include terminal blocks, bearings, bushings, control cams, electrical connectors, housings, cable ties, fasteners, switch components and industrial parts that require chemical resistance, stiffness, wear resistance and rigidity.Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh RigidityHigh StrengthLubricatedOil ResistantSolvent ResistantUses:BearingsBushingsCamsConnectorsHousingsIndustrial ApplicationsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm

@Diameter 2.00 mm
0.017 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-2
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Elongation at Yield 25 %
25 %
ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-2
Flexural Strength 50.0 MPa
7250 psi
ISO 178
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180
20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA