Ascend Performance Materials Vydyne® 00XFS Nylon 66/6 Copolymer

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 00XFS Nylon 66/6 Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 00XFS maintains the chemical resistance typical of PA66/6 to many chemicals, machine and motor oils, solvents and gasoline. Typical Applications/End Uses: CompoundingAvailability:Asia PacificEuropeNorth America Features:CopolymerGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical Resistance Good ToughnessHigh RigidityHigh StrengthOil ResistantSolvent ResistantUses:CompoundingGeneral PurposeAppearance: Natural ColorForms: PelletsProcessing Method: Compounding and Compounding ExtrusionInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Bulk Density 0.674 g/cc
0.0243 lb/in³
ASTM D1895
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption 0.500 %
0.500 %
ASTM D6869
Relative Viscosity 45 - 51 cP
45 - 51 cP
Formic Acid; ASTM D789
Viscosity Measurement 137 - 148
137 - 148
Viscosity Number cm³/g; H2SO4; ISO 307
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ISO 11357-3
Optical Properties Metric English Comments
Yellow Index -4.00 %
-4.00 %
ASTM D1925