Asahi Kasei Thermylon® LSG-440A-H 60% Ceramic and Glass Fiber Reinforced, Heat

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Asahi Kasei
Trade Name Thermylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylon® LSG-440A-H 60% Ceramic and Glass Fiber Reinforced, Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 193 MPa
28000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 290 MPa
42000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm
16.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 268 °C
515 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
485 °F
ASTM D648