Asahi Kasei Thermylene® P-15FG-0860 15% Glass Fiber Reinforced, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P-15FG-0860 15% Glass Fiber Reinforced, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm
9.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 48.6 µm/m-°C

@Temperature 20.0 °C
27.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Flammability, UL94 HB
HB
0.0591 in thickness