Material Notes:
20% Mineral filled, high stiffness, low warp gradeInformation provided by Asahi Kasei Corporation.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Asahi Kasei Method
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133 D
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.0 MPa
8850 psi
ISO 527 - 1 & - 2
Elongation at Break 5.0 %
5.0 %
ISO 527 - 1 & - 2
Tensile Modulus 4.90 GPa
711 ksi
ISO 527 - 1 & - 2
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 / 1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 161 °C
322 °F
ISO 75 -1 & -2 flat
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
268 °F
ISO 75 -1 & -2 flat
Flammability, UL94 HB
HB