Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Secure™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Secure™ Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell EncapsulationDesign/Construction:Liner: 2.5 mil PolyethyleneSide 1: Uncured RubberSubstrate: 1080 Style FiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
432 microns
17.0 mil
Silicone; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa

@Strain <=1.00 %
3550 psi

@Strain <=1.00 %
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 125 %
125 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Peel Strength 0.351 kN/m
2.00 pli
Bond Strength (S1 to S1); Arlon SQA-TMS-024
Thermal Properties Metric English Comments
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E831
Specific Heat Capacity 0.820 J/g-°C

@Temperature 100 °C
0.196 BTU/lb-°F

@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E1530
Maximum Service Temperature, Inert 204 °C
399 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -118 °C
-180 °F
Silicone Property; ASTM D3418
UL RTI, Electrical 150 °C
302 °F
UL RTI, Mechanical without Impact 150 °C
302 °F
Flammability, UL94 V-0
V-0
E54153
Electrical Properties Metric English Comments
Dielectric Constant 6.9

@Frequency 1.00e+6 Hz
6.9

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
Dielectric Strength 31.9 kV/mm
810 kV/in
ASTM D149
Dissipation Factor 0.0044

@Frequency 1.00e+6 Hz
0.0044

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
Processing Properties Metric English Comments
Shelf Life 3.00 Month

@Temperature 7.22 °C
3.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color Gray
Silicone
White
Substrate
Plasticity (mm) 2.3
Arlon SQA-TMS-005; Silicone Property