Material Notes:
Cured silicone rubber with a minimum thickness of 0.027 in. (0.69 mm)/0.018 in. (0.46 mm) Prime Coated 162 Fiberglass/Cured silicone rubber with a minimum thickness of 0.017 in. (0.43 mm); 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.062 in ±0.005 (1.6 mm ± 0.1). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 2299 g/m² ± 187 (67.8 oz./yd.² ± 5.5).Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 4.32 - 5.28 MPa
627 - 766 psi
Elongation at Break 315 - 385 %
315 - 385 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
continuous