Material Notes:
Fully cured, unsupported, static dissipating silicone.Design/Construction:Liner: 3 mil PolyethyleneProduct: Fully Cured Silicone RubberCarrier: N/AThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Arlon SQA-TMS-024
Thickness 1270 microns
50.0 mil
Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength 4.83 MPa
700 psi
ASTM D412
Elongation at Break 290 %
290 %
ASTM D412
Compression Set 25 %
25 %
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Black
Total Product Weight (oz/yd2) 44.6
Arlon SQA-TMS-025