Arlon R34710R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&l

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R34710R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&l.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: 20 mil thick uncured, uncatalyzed silicone rubber. Used for sealing biochemical reaction chambers.Design/Construction:Liner: Polyethylene Product: Uncured Silicone Rubber Carrier: Mylar This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Carrier
76.2 microns
3.00 mil
Liner
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 18.3 - 23.9 °C
6.00 Month

@Temperature 65.0 - 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Clear
Pink
Liner
Total Product Weight (oz/yd2) 18
Arlon SQA-TMS-025