Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Static dissipating siliconeDesign/Construction:Interleave: 0.0025" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Carrier; Arlon SQA-TMS-003
381 microns
15.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 4.83 MPa
700 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 290 %
290 %
Silicone Property; Arlon SQA-TMS-008
Tear Strength 12.3 kN/m
70.0 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Black
Total Product Weight (oz/yd2) 13.4
Arlon SQA-TMS-025