Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape

Category Polymer , Tape , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The following tests are conducted on one roll from each lot of tape per Mil-I-46852C: Thickness, Width, Bond Strength, Tensile Strength, Elongation, Dielectric Strength, and Water Absorption.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Silicone Property; Arlon SQA-TMS-024
Water Absorption 2.8 %
2.8 %
MIL-I-46852C
Thickness 508 microns
20.0 mil
Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength, Ultimate 7.93 MPa
1150 psi
Silicone Property; ASTM D412
Elongation at Break 430 %
430 %
Silicone Property; ASTM D412
Adhesive Bond Strength 0.0214 MPa
3.10 psi
MIL-I-46852C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following: