Material Notes:
1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Design/Construction:Interleave: 2.5 mil PolyethyleneRubber: Cured Self-fusing Silicone RubberCross-section: 1" wide rectangularThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.0 %
1.0 %
Arlon SQA-TMS-016
Thickness 508 microns
20.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 7.674 MPa
1113 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 462 %
462 %
Silicone Property; Arlon SQA-TMS-009
Peel Strength 0.596 kN/m
3.40 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 27.6 kV/mm
701 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Brown
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved