Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Side 1 Silicone Property; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Side 2 Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
178 microns
7.00 mil
Side 2; Arlon SQA-TMS-003
406 microns
16.0 mil
Substrate; Arlon SQA-TMS-003
635 microns
25.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Side 1 Silicone Property; ASTM D2240
60
60
Side 2 Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Side 1 Silicone Property; ASTM D412
6.21 MPa
900 psi
Side 2 Silicone Property; ASTM D412
Elongation at Break 200 %
200 %
Side 1 Silicone Property; ASTM D412
300 %
300 %
Side 2 Silicone Property; ASTM D412
Peel Strength 1.31 kN/m
7.50 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle; under pressure
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 29
Arlon SQA-TMS-025