Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat) Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Side 2, Layer 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
292 microns
11.5 mil
Side 2, Layer 2; Arlon SQA-TMS-003
483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
813 microns
32.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Silicone Property; ASTM D2240
Tensile Strength 7.58 MPa
1100 psi
Silicone Property; ASTM D412
Elongation at Break 650 %
650 %
Silicone Property; ASTM D412
Peel Strength 4.21 kN/m
24.0 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
E54153
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Electrical Properties Metric English Comments
Dielectric Strength 20.9 kV/mm
530 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Total Product Weight (oz/yd2) 31
Arlon SQA-TMS-025