Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 51268R015P 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51268R015P 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
152 microns
6.00 mil
Side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Silicone Property; ASTM D2240
Tensile Strength 6.07 MPa
880 psi
Silicone Property; ASTM D412
Elongation at Break 480 %
480 %
Silicone Property; ASTM D412
Tear Strength 11.0 kN/m
63.0 pli
ASTM D624
Peel Strength 1.51 kN/m
8.60 pli
Bond Strength; Arlon-SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm
560 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 16.7
Arlon SQA-TMS-025