Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 3.0 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Holland ClothThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
1570 microns
62.0 mil
Silicone; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Silicone Property; ASTM D2240
Tensile Strength 7.58 MPa
1100 psi
Silicone Property; ASTM D412
Elongation at Break 400 %
400 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 54.8
Arlon SQA-TMS-025