Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Interleave
127 microns
5.00 mil
Carrier
762 microns
30.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Elongation at Break 700 %
700 %
Silicone Property; ASTM D412
Tear Strength 35.1 kN/m
200 pli
Silicone Property; ASTM D624
Compression Set 28 %
28 %
Silicone Property; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 177 °C
0.500 hour

@Temperature 350 °F
Recommended Cure Cycle
240 min

@Temperature 227 °C
4.00 hour

@Temperature 440 °F
Recommended Postcure Cycle
Shelf Life 3.00 Month

@Temperature 7.22 °C
3.00 Month

@Temperature 45.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally Translucent
Total Product Weight (oz/yd2) 27
Arlon SQA-TMS-025