Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 32210A005 0.005" (0.127 mm) Uncured Fluorosilicone Rubber on Polyester Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 32210A005 0.005" (0.127 mm) Uncured Fluorosilicone Rubber on Polyester Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone RubberCarrier: PolyesterThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Overall; Arlon SQA-TMS-003
127 microns
5.00 mil
Side 1; Arlon SQA-TMS-003
127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Silicone Property; ASTM D2240
Tensile Strength 7.453 MPa
1081 psi
Silicone Property; ASTM D412
Elongation at Break 83 %
83 %
Silicone Property; ASTM D412
Tear Strength 7.19 kN/m
41.0 pli
Die B, Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 51.81 kV/mm
1316 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Clear
Carrier
Light Gray
Fuel Resistance 0.118
Fuel CM85, ASTM D471(tested at 65°C for 48 hr)
0.139
Fuel A, ASTM D471(tested at 20°C for 24 hr)
0.269
Fuel C, ASTM D471(tested at 65°C for 48 hr)
Total Product Weight (oz/yd2) 8.5