Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneProduct: Uncured Fluorosilicone Rubber Carrier: Release coated HDPE Product Use: Flexible heater insulationAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
508 microns
20.0 mil
Side 1; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Elongation at Break 225 %
225 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 200 °C
392 °F
E54153
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 45.75 kV/mm
1162 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Translucent
Carrier
Total Product Weight (oz/yd2) 18.6
Arlon SQA-TMS-025