Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Side 2; Arlon SQA-TMS-024
1.56 g/cc
0.0564 lb/in³
Side 1; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
102 microns
4.00 mil
Side 1; Arlon SQA-TMS-003
178 microns
7.00 mil
Side 2; Arlon SQA-TMS-003
356 microns
14.0 mil
Substrate; Arlon SQA-TMS-003
635 microns
25.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
Side 2; ASTM D2240
55
55
Side 1; ASTM D2240
Tensile Strength 3.65 MPa
530 psi
Side 1; ASTM D412
6.55 MPa
950 psi
Side 2; ASTM D412
Elongation at Break 300 %
300 %
Side 1; ASTM D412
620 %
620 %
Side 2; ASTM D412
Tear Strength 7.01 kN/m
40.0 pli
Side 1; ASTM D624
26.3 kN/m
150 pli
Side 2; ASTM D624
Peel Strength 2.98 kN/m
17.0 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB

@Temperature 200 °C
HB

@Temperature 392 °F
per card E54153
Electrical Properties Metric English Comments
Dielectric Strength 13.8 kV/mm
350 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 28.8
Arlon SQA-TMS-025