Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Fluorinated Ethylene Propylene Interleave
38.1 microns
1.50 mil
Mylar Carrier
584 - 686 microns
23.0 - 27.0 mil
Overall
584 - 686 microns
23.0 - 27.0 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 75
65 - 75
Compound Property
Tensile Strength >= 7.93 MPa
>= 1150 psi
Compound Property
Elongation at Break >= 300 %
>= 300 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally Translucent
Total Product Weight (oz/yd2) 21.8 - 25.8