Product Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 2290 microns
90.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength >= 6.89 MPa
>= 1000 psi
Elongation at Break >= 700 %
>= 700 %
Tear Strength >= 35.1 kN/m
>= 200 pli
Compression Set <= 28 %
<= 28 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Descriptive Properties Value Comments
Total Product Weight (oz/yd2) 75.7