Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
457 - 559 microns
18.0 - 22.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Compound Property
Tensile Strength >= 6.89 MPa
>= 1000 psi
Compound Property
Elongation at Break >= 700 %
>= 700 %
Compound Property
Tear Strength >= 35.1 kN/m
>= 200 pli
Compound Property
Compression Set <= 28 %
<= 28 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Descriptive Properties Value Comments
Color Saddle Brown
Total Product Weight (oz/yd2) 14.8-18.8