Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon.Example applications: Oil tank, hydraulic fluid tank.ISO data provided by the manufacturer, Arkema.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 35 %
35 %
50 mm/min
Tensile Modulus 0.525 GPa
76.1 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 5.17 J/cm²
24.6 ft-lb/in²
2.42 J/cm²

@Temperature -30.0 °C
11.5 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
Vicat Softening Point 146 °C
295 °F
50°C/hr; 50N