Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical resistance.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 2.7 %
2.7 %
Moisture Absorption at Equilibrium 1.2 %
1.2 %
Humidity Absorption
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Tensile Modulus 1.66 GPa
241 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.05 J/cm²

@Temperature -30.0 °C
5.00 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °C
147 °F
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
Vicat Softening Point 67.0 °C
153 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.