Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Cable Sheathing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be processed for injection molding and sheathing of cables. Low shrinkage for molding: include 1% on average for the mold design.UL classification: UL94 V0 (3mm) RTI(C) 65/65/65Example applications: Electrical cables, all pieces with fireproofing required.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Water Absorption 1.96 %
1.96 %
Moisture Absorption at Equilibrium 0.64 %
0.64 %
Humidity Absorption
Melt Flow 95.1 g/10 min

@Load 2.16 kg,
Temperature 235 °C
95.1 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 2.07 GPa
300 ksi
1 mm/min
Charpy Impact Unnotched 0.850 J/cm²

@Temperature -30.0 °C
4.05 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 102 µm/m-°C

@Temperature 20.0 °C
56.7 µin/in-°F

@Temperature 68.0 °F
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Oxygen Index 33 %
33 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Strength 28.5 kV/mm
724 kV/in
Dissipation Factor 0.000315

@Frequency 1e+6 Hz
0.000315

@Frequency 1e+6 Hz
0.000328

@Frequency 100 Hz
0.000328

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: