Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold. High dimensional stability due to its low moisture absorption.Potable water contact approval WRC 940 7502.Example applications: All sort of pieces for food applications.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Water Absorption 1.9 %
1.9 %
Melt Flow 8.8 g/10 min

@Load 2.16 kg,
Temperature 235 °C
8.8 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 1.58 GPa
229 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 0.730 J/cm²
3.47 ft-lb/in²
0.990 J/cm²

@Temperature -30.0 °C
4.71 ft-lb/in²

@Temperature -22.0 °F