Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength. Good fatigue resistance. Good chemical resistance.Example applications: Pneumatic applications.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Moisture Absorption at Equilibrium 0.70 %
0.70 %
Humidity Absorption
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.165 GPa
23.9 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
10°C/min
Deflection Temperature at 1.8 MPa (264 psi) 36.0 °C
96.8 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Users viewing this material also viewed the following: