Material Notes:
Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. Well adapted melt viscosity. Ability to be processed in thin wall thickness. Easy to color.Example applications: Coating of electrical and telephone cable.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Water Absorption 1.5 %
1.5 %
Melt Flow 27.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
27.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 1.86 GPa
270 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 30 %
30 %
Electrical Properties Metric English Comments
Dissipation Factor 0.000306

@Frequency 100 Hz
0.000306

@Frequency 100 Hz
0.000316

@Frequency 1e+6 Hz
0.000316

@Frequency 1e+6 Hz