Material Notes:
Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon.Example applications: Oil tank, hydraulic fluid tank.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Water Absorption 1.6 %
1.6 %
Moisture Absorption at Equilibrium 0.70 %
0.70 %
Humidity Absorption
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 9.0 %
9.0 %
50 mm/min
Tensile Modulus 1.24 GPa
180 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F