Material Notes:
Plexiglas® DR® M2 is an impact modified thermoplastic acrylic resin formulated for injection molding and extrusion applications. It has a matte appearance, is heat resistance and provides 10 times the impact resistance of standard acrylics. It offers an excellent balance between melt flow and increased resistance to breakage, while providing weatherability superior to that provided by other high-impact plastics.Appearance: Matte Finish; Clear/TransparentCharacteristics: Scratch Resistant; Good Dimensional Stability; Low Shrinkage; Good Thermal Stability; Good UV Resistance; Good Weather Resistance; Good Toughness; High Impact Resistance
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 1.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 2.5 %

@Thickness 3.17 mm
2.5 %

@Thickness 0.125 in
ASTM D1003
Transmission, Visible 88 %

@Thickness 3.17 mm
88 %

@Thickness 0.125 in
ASTM D1003