Material Notes:
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).Suited to the extrusion of tubes (hydraulic, pneumatic, painting...). Also for injection molding.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Water Absorption 5.5 %
5.5 %
Moisture Absorption at Equilibrium 1.5 %
1.5 %
Humidity Absorption
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 7.0 %
7.0 %
50 mm/min
Tensile Modulus 0.800 GPa
116 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V