Material Notes:
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).lower in viscosity than LE 6000. Suited to cast film extrusion. Injection molding is also possible.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V