Arkema Group Orevac® OE807 Maleic Anhydride modified LLDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orevac® OE807 Maleic Anhydride modified LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Orevac® OE807 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers. Orevac® OE807 is characterized by a high level of maleic anhydride.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.911 g/cc
0.0329 lb/in³
ASTM D1505
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 810 %
810 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
D.S.C. method
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525-82