Material Notes:
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Vinyl Acetate Content 23.5 - 26.5 %
23.5 - 26.5 %
Melt Flow 5.5 - 9.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 - 9.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 29.2
29.2
ISO 868
Tensile Strength at Break 25.9 MPa
3760 psi
50 microns film; ASTM D882
Tensile Strength, Yield 4.20 MPa
609 psi
50 microns film; ASTM D882
Elongation at Break 730 %
730 %
50 microns film; ASTM D882
Modulus of Elasticity 0.0264 GPa
3.83 ksi
ISO R527
Dart Drop Test 400 g
0.882 lb
50 microns film
Thermal Properties Metric English Comments
Melting Point 77.0 °C
171 °F
D.S.C. method
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 4.6 %
4.6 %
50 micron film; ASTM D1003