Arkema Group Nakan® FMS 801 L PVC, Soft Injection Molding Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Arkema
Trade Name Nakan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Nakan® FMS 801 L PVC, Soft Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NAKAN FMS 801 L is a soft polyvinyl chloride compound developed for injection molding of safety spectacles and for various applications.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.00 MPa

@Strain 50.0 %
580 psi

@Strain 50.0 %
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.