Arkema Group Lucalor® PEY 221 CPVC, Pipe Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC)
Manufacturer Arkema
Trade Name Lucalor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lucalor® PEY 221 CPVC, Pipe Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LUCALOR PEY 221 is a chlorinated polyvinyl chloride compound (CPVC) developed for the extrusion of pipes for hot water supply and distribution systems.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
50 mm/min
Elongation at Break 23 %
23 %
Nominal Strain; 50 mm/min
Elongation at Yield 4.0 %
4.0 %
50 mm/min
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 1.01 J/cm²
4.81 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Vicat Softening Point 115 °C
239 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 75 %
75 %